<1> The application of MC nylon MC nylon uses widely in the project plastic at now, particularly in the machine aspect for reducing bearing whetting aterial to replace alloy and copper material . 1,The machine strength is high, the tenacity is big, the bearing to whet is good, the fusion point is high, and bear the oil, bear the eclipse, bear the water. 2,The size stability is good, can lubricant itself and is not restricted by its size. 3,The cost is low, the life span is long, and the cost is only for metals’s 50%-70%, life span is general longer 2-3 times than metal’s.The use of MC nylon is very wide, such as turbine, wheel gear, silk pole etc on the machine <2> Phisical property |
 |
| Item |
Unit |
Casting nylon |
| Tensile strength |
Kgf/cm2 |
916-890(900) |
| Bending strength |
Kgf/cm2 |
1586-1547(1550) |
| Compression strength |
Kgf/cm2 |
1068-1400(1115) |
| Shear strength |
|
740-810 |
| Impact(No notch) |
Kgf.cm/cm2 |
520-624(145) |
| Hardness |
RH R-ST.BH |
R110-120M91-M88 |
| Elongation ratio |
% |
10~30 |
| Expansion elastic modulus |
Kgf/cm2 |
40x103 |
| Bending elastic modulus |
oC |
40x103 |
| Fusion point |
|
223-225oC |
| Density |
g/cm3 |
1.15-1.16 |
| Saturation mean molecular weight in 24h |
% |
0.9 |
| 5-10x104 |
| Matin heatproof |
oC |
67-74oC |
| liner expansion coefficient |
X105/oC |
8.3-7.6 |
| Specific heat volume |
Kcal/kg.oC |
150-190 |
| Coefficient of thernal conductivity |
Kcal/m.h.oC |
0.28-0.29 |
| Sparking voltage |
Kv/mm |
15-23.6 |
| Volume resistivity |
Qu-cm |
3.4 |
| Electrolytic constant |
loss 150Hz lower than 10.6 |
4.5x10-3 |
| Electrolitic loss |
150Hz |
1.5-2.0x10-3 | |